| 1. | Anti penetration of hardened mortar can reach 10 - 7cm / s . adopting sulfate - aluminum cement , phosphorus slag , flying ash , yellow slag and ect raw materials , the optimized mixture program of dmm is a3b3c2 ( cement 480 m2 / kg , phosphorus slag352 m2 / kg , activated agent 3 % ) , 28 strength is low , due to cement alkality , resulting in activity of phosphorus slag and flying ash small 采用硫铝酸盐水泥,磷渣、粉煤灰、黄砂等原武汉理工大学硕士学位论文料配制抗渗干拌砂浆最优配料方案为: a3b3c2 (水泥比表面积4som , / kg ,磷渣比表面积352mz / kg ,激发剂3 % ) 。 |